Correct Answer:
Option A - It has high lime content can be obtained by increasing the C₃S content but is normally obtained from OPC clincker by finer grinding.
Tricalcium silicate (C₃S) [25-50%]– It increase the resistance to freezing and thawing.
• It is responsible for early strength and hardness.
• The heat of hydration is 500 J/g.
Tricalcium aluminate (C₃A) [5-11%]–
• It rapidly leads with water and is responsible for flash set to finely grounded clinker.
• C₃A is responsible for the initial setting.
• The heat of hydration of 865 J/g.
A. It has high lime content can be obtained by increasing the C₃S content but is normally obtained from OPC clincker by finer grinding.
Tricalcium silicate (C₃S) [25-50%]– It increase the resistance to freezing and thawing.
• It is responsible for early strength and hardness.
• The heat of hydration is 500 J/g.
Tricalcium aluminate (C₃A) [5-11%]–
• It rapidly leads with water and is responsible for flash set to finely grounded clinker.
• C₃A is responsible for the initial setting.
• The heat of hydration of 865 J/g.